Hostacom HYG 400-2L NAT is a 20% glass fiber reinforced PP homopolymer, with outstanding flowability and good surface appearance. Product is available as natural, pellet form. Product is UL listed. This grade is not intended for medical, pharmaceutical, food or drinking water applications. This grade is delivered in NAT color version. Dry material before processing.Information provided by LyondellBasell. |