Westlake EF612 is an LDPE resin suggested for use in films requiring good clarity and toughness. It has excellent process ability, and is an excellent choice as a blend resin with LLDPE in general-purpose clarity packaging applications. Test specimens for blown film: nominal thickness 1.25 mils; blow up ratio 2.5:1, die gap 35 mils at 50% relative humidity and 23°C. Information provided by Westlake Chemical. |