MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Zircar Zirconia ALF-100 Alumina Felt Insulation
Categories: Ceramic; Machinable Ceramic; Oxide; Aluminum Oxide

Material Notes: Alumina (Al2 O3) has excellent thermal shock resistance, high dimensional stability and good chemical inertness, which makes our alumina fiber products ideal for fast firing cycles up to 1700°C. Our alumina fibers and textiles are made by the same unique Zircar process used for manufacturing yttria-stabilized zirconia cloths and felts. This process yields a high purity alumina fiber with only trace amounts of silica, making it more stable in hydrogen environments than the more commonly found sol-gel alumina fibers that have 3% silica. Our high purity alumina fiber and textiles are offered in six different standard product forms bulk fiber Type ALBF, two felts Types ALF-50 and ALF-100 and three types of knit cloth Types ALK-15, ALW-15 and ALW-30.

Features:

  • Excellent Thermal Shock Resistance
  • 99% Pure Alumina
  • Trace Level of Silica (0.09 wt%)
  • Dimensional Stability in Hydrogen
  • Low Thermal Conductivity
  • No Outgassing
  • Six Different Product Formats Offered
  • Available ‘Off the Shelf’

Application Information:

  • Alumina fiber textiles are used as insulation for glass melting furnaces.
  • Alumina bulk fiber, Type ALBF, is used as bulk fill insulation.
  • Alumina fiber textiles are used as insulation for fiber optic furnaces.
  • Alumina fiber textiles are used in SOFC and PEM type fuel cells as gaskets.
  • Alumina fiber cloth is used as insulation in differential scanning calorimeters (DSC’s).

Information provided by Zircar Zirconia.

Key Words: Al2O3, aluminum oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.130 g/cc
Loss On Ignition 3.8 %
@Temperature 950 °C,
Time 3600 sec
Porosity 97 %Bulk
Outgassing - Total Mass Loss 0.00 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 2015 °C
Shrinkage 15 %
@Temperature 1650 °C,
Time 3600 sec
 
Component Elements PropertiesOriginal ValueComments
Al2O3 >= 99 %
CaO 0.060 %
SiO2 0.090 %
ZrO2+Y2O3 0.42 %
 
Descriptive Properties
Tensile Strength per Unit Width49 gram/cm width

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Alumina, alpha Al2O3, 99.5%
MarkeTech Aluminum Oxide Ceramic - Alumina 96%
Overview - Alumina, 96%, Al2O3
Anderman Ceramics EA99P Sintered Alumina, 99%, Porous
Magnesia Stabilized Zirconia

C6ZIR026 / 2782

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.