EVATANE® 33-45 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 33-45 is stabilized with antioxidants. The High Vinyl Acetate content of EVATANE® 33-45 brings softness, flexibility and polarity. EVATANE® 33-45 is compatible with tackifying resins and waxes. It’s a useful product for hot melt adhesives formulation. EVATANE® 33-45 delivers high cohesive strength with any kind of fillers (HFFR compounds). It can also be used as an additive for crude oil (pour point depressant) or bitumen.Information provided by Arkema Group |