MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Aurora Plastics TufTech™ 5501124 Vinyl
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Application: Replacement for TPV/TPR materials for application requiring an excellent compression set properties, Weatherable, Elastomeric, Extrusion Molding Compound. Targeting for GMP PVC 088.

Information provided by S&E Specialty Polymers; S&E Specialty Polymers was aquired by Aurora Plastics in 2017.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 55
@Time 15.0 sec
ISO 868
Tensile Strength at Break 1120 psi
Elongation at Break 450 %500mm/min; ISO 257, 1A
Tear Strength 59.3 pliMethod B, angle die, 500mm/min.; ISO 34-1
Compression Set 15 %
@Temperature 24.0 °C,
Time 86400 sec
ISO 815-1, Type A
 35 %
@Temperature 70.0 °C,
Time 79200 sec
ISO 815-1, Type A
 35 %
@Temperature 100 °C,
Time 252000 sec
ISO 815-1, Type A
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air -34.0 °CCold Flex; No cracks, 6 mm mandrel; SAE J323, Method A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Softell CA7469A Thermoplastic Olefinic Elastomer

PSEPN032 / 179036

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.