MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Celanese Hytrel® HTR8441 BK316 TPC-ET
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: 55 Shore D High Viscosity Polyester Elastomer Developed for Blow Molding

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccISO 1183
Melt Density 1.01 g/cc
@Temperature 245 °C
Linear Mold Shrinkage, Flow 0.022 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.021 cm/cmISO 294-4, 2577
Melt Flow 9.0 g/10 min
@Load 10.0 kg,
Temperature 240 °C
cm³/10min Volumetric; ISO 1133
 9.0 g/10 min
@Load 10.0 kg,
Temperature 240 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 5215s; ISO 48-4
 <= 56ISO 48-4
Tensile Stress at Strain 8.00 MPa
@Strain 5.0 %
1BA specimen at 50mm/min; ISO 527-1/-2
 13.0 MPa
@Strain 10 %
ISO 527-1/-2
 19.0 MPa
@Strain 50 %
ISO 527-1/-2
Tensile Modulus 190 MPaISO 527-1/-2
Flexural Modulus 190 MPaISO 178
Poissons Ratio 0.48
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 19.0 kJ/m²
@Temperature -40.0 °C
ISO 179/1eA
 39.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 NB
@Temperature 23.0 °C
ISO 179/1eA
Tensile Impact Strength 330 kJ/m²
@Temperature 23.0 °C
Notched; ISO 8256/1
Tear Strength 135 kN/mnormal; ISO 34-1
 150 kN/mparallel; ISO 34-1
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 2.15 J/g-°C
@Temperature 245 °C
Melt
Thermal Conductivity 0.160 W/m-K
@Temperature 245 °C
Melt
Melting Point 214 °C10°C/min; ISO 11357-1/-3
Brittleness Temperature -54.0 °CISO 974
Glass Transition Temp, Tg -40.0 °C10°C/min; ISO 11357-1/-2
Flame Spread 42.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 225 - 240 °CRange, Extrusion
 230 - 240 °CRange, Blow Molding
 235 °COptimum, Blow Molding
 245 °COptimum, Injection
 240 - 255 °CRange, Injection
Mold Temperature 45.0 °COptimum, Blow Molding
 45.0 °COptimum, Injection
 40.0 - 55.0 °CInjection
 40.0 - 60.0 °CRange, Blow Molding
Drying Temperature 100 °CInjection
 100 - 110 °CBlow Molding
 110 °CExtrusion
Dry Time 2.00 - 3.00 hourExtrusion, Dehumidified Dryer
 2.00 - 4.00 hourInjection, Dehumidified Dryer
 4.00 - 6.00 hourBlow Molding, Dehumidified Dryer
Moisture Content <= 0.030 %Blow Molding
 <= 0.060 %Extrusion
 <= 0.080 %Injection
 
Descriptive Properties
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
Odor Class3.5VDA 270; DS
Part Marking Code>TPC-ET<ISO 11469
PolymerTPC
Resin IdentificationTPC-ETISO 1043
Swell ratio2.4Blow Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Hytrel® HTR8206 TPC-ET
Celanese Hytrel® 8238 TPC-ET
Celanese Hytrel® HTR8223 BK320 TPC-ET
Celanese Hytrel® HTR8341C BK320 TPC-ET
Celanese Hytrel® HTR8685 BK022A TPC-ET

PDSX5216 / 197856

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.