MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Go Yen Chemical High-Strength Plastic Rubber Anti-Precipitation Reinforcing Agent Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Not only has excellent reinforcement, whiteness; and have good plasticity and high adhesion, can make rubber processing manufacturing process to prevent plasticized oil, plasticizing agents and aromatic hydrocarbon white oil, silicon oil precipitation (migration).

Advantages:

  • Outstanding additives for rubber
  • Excellent reinforcing agent
  • Good whiteness
  • Excellent processing ability
  • Good oil absorption after mixed with plastic and rubber
  • Prevent rubber migration
  • Excellent insulation properties
  • Anti-acid solubility
  • Heat resistance
  • High added value for products
  • Prevent the migration of plasticizing oil, plasticizer and aromatic hydrocarbon white oil, silicon oil
Applications:
  • Rubber industry(CR, NR, SBR, EPDM, HYPALON)
  • Rubber and rubber tile
  • Waterproof tape
  • Can be used in rubber material of high tension , high mold and high hardness
  • Rubber shoes soles and heel
  • PVC window frames, wire and cable
  • Paint and Latex paint for mental interior pipe
  • Back glue for carpet
  • Paint industry( all kinds of decorated, interior, external coating
  • Ceramics industries ( aeronautical technology and various additives for industry field)

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.60 g/cc
Particle Size 75 µm
pH 5.3 - 6.3
 
Processing PropertiesOriginal ValueComments
Moisture Content 1.0 %
 
Descriptive Properties
Oil Absorption69-79 g/100g
Whiteness78 GBE

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN407 / 266715

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.