MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Corning G 50 Tinted Optical Glass
Categories: Ceramic; Glass; Optical

Material Notes: Application : Pass cited standards for traffic signal recognition at 1.9 mm thickness 100 % UV absorbing glass suited for general or special purpose Tinted glass.

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.48 g/cc
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.74 µm/m-°C
Softening Point 645 °C
Annealing Point 492 °C
Strain Point 645 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.52061
@Wavelength 656.3 nm
Line: C; Hydrogen
 1.52102
@Wavelength 643.8 nm
Line: C'; Cadmium
 1.52328
@Wavelength 587.6 nm
Line: d; Helium
 1.52532
@Wavelength 546.1 nm
Line: e; Mercury
 1.52926
@Wavelength 486.1 nm
Line: F; Hydrogen
 1.52974
@Wavelength 480 nm
Line: F'; Cadmium
Abbe Number 60.24ve
 60.49vd
Transmission, Visible 49.6 %
@Wavelength 380 - 780 nm,
Thickness 1.90 mm
Luminous
 50 %
@Wavelength 380 - 500 nm,
Thickness 1.90 mm
Blue light transmission factor
UV Transmittance <= 0.10 %
@Wavelength 280 - 315 nm,
Thickness 1.90 mm
UV - B t?(max)
 <= 0.10 %
@Wavelength 280 - 315 nm,
Thickness 1.90 mm
t(avg)
 <= 0.10 %
@Wavelength 315 - 350 nm,
Thickness 1.90 mm
Solar UV-B transmission factor
 <= 0.10 %
@Wavelength 315 - 350 nm,
Thickness 1.90 mm
UV - A t?(max)
 <= 0.10 %
@Wavelength 380 - 500 nm,
Thickness 1.90 mm
t(avg)
 <= 0.10 %
@Wavelength 380 - 500 nm,
Thickness 1.90 mm
Solar UV-A transmission factor
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Corning N-BX 15 Tinted Optical Glass
Corning ULE® 7973 Premium Grade Ultra Low Expansion Glass
Corning GREY 17 Tinted Optical Glass
Corning FUSIBLE PHOTOGRAY THIN&DARK ™ Wide range photochromic glass for thin lenses
Corning Eagle XG® Slim Display Glass

CCORN916 / 233327

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.