LNP LUBRICOMP DCL32 compound is based on Polycarbonate (PC) resin containing 10% carbon fiber and 15% PTFE. Added features of this grade include: Wear Resistant, Electrically Conductive. Features: Wear resistant,Electrically Conductive,Structural Information provided by SABIC |