MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC CYCOLOY™ FR CY6310 PC+ABS (Asia)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: CYCOLOY CY6310 Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS) blend is an impact modified, high flow and heat resistant, injection moldable, non chlorinated/brominated flame retardant grade. It has a UL94 V0@1.5mm, 5VA@2.9 and 5VB@2.3mm flame rating. This grade is an excellent candidate for a variety of large size applications.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.17 g/ccASTM D792
Density 1.17 g/ccISO 1183
Water Absorption 0.60 %23°C/sat; ISO 62
Moisture Absorption 0.200 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 16 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ASTM D1238
 19 g/10 min
@Load 2.16 kg,
Temperature 260 °C
cm³/10 min; ISO 1133
 20 g/10 min
@Load 2.16 kg,
Temperature 260 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 50.0 MPa50 mm/min; ASTM D638
 51.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 63.0 MPa50 mm/min; ISO 527
 63.0 MPa50 mm/min; ASTM D638
Elongation at Break >= 50 %50mm/min; ISO 527
 >= 50 %50mm/min; ASTM D638
Elongation at Yield 4.2 %50 mm/min; ASTM D638
 4.4 %50 mm/min; ISO 527
Tensile Modulus 2700 MPa5 mm/min; ASTM D638
 2700 MPa1mm/min; ISO 527
Flexural Yield Strength 91.0 MPa2 mm/min; ISO 178
 101 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2650 MPa2 mm/min; ISO 178
 2700 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 600 J/mASTM D256
 115 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 50.0 kJ/m²80*10*3; ISO 180/1A
 13.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*3; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 55.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 14.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 65.0 JASTM D3763
Impact Test 105 JMultiaxial Impact; ISO 6603
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Comparative Tracking Index 575 VIEC 60112
Hot Wire Ignition, HWI 15 - 30 secUL 746A
High Amp Arc Ignition, HAI >= 120 arcsUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 68.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 68.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Hot Ball Pressure Test 100 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 88.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 109 °CRate B/50; ASTM D1525
 109 °CRate B/50; ISO 306
 111 °CRate B/120; ISO 306
UL RTI, Electrical 85.0 °CUL 746B
UL RTI, Mechanical with Impact 85.0 °CUL 746B
UL RTI, Mechanical without Impact 85.0 °CUL 746B
Flammability, UL94 V-2
@Thickness 0.750 mm
UL 94
 V-2
@Thickness 0.750 mm
UL 94 by SABIC-IP
 V-0
@Thickness 1.50 mm
UL 94 by SABIC-IP
 V-0
@Thickness 1.50 mm
UL 94
 5VB
@Thickness 2.30 mm
UL 94
 5VB
@Thickness 2.30 mm
UL 94 by SABIC-IP
 5VA
@Thickness 2.90 mm
UL 94
 5VA
@Thickness 2.90 mm
UL 94 by SABIC-IP
Oxygen Index 30 %ISO 4589
Glow Wire Test 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °CHopper Temperature
Nozzle Temperature 230 - 270 °CInjection Molding
Zone 1 210 - 240 °C
Zone 2 230 - 270 °C
Zone 3 240 - 280 °C
Melt Temperature 250 - 280 °C
Mold Temperature 60.0 - 90.0 °C
Drying Temperature 90.0 - 100 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10800 / 244267

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.