MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kumho-Sunny XC811-HW ASA
Categories: Polymer; Thermoplastic; ASA Polymer; Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded

Material Notes: ASAXC811 is a type of high heat-resistance grade of ASA resin, with better weatherability than ASA XC811, high rigidity and toughness.

Application: Automotive exteriors like radiator grille, pillar board, rearview mirror, license plate board, etc.

Information provided by Shanghai Kumho Sunny Plastics co, Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.09 g/ccISO 1183
Maximum Moisture Content 0.050
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmISO 294
Melt Flow 5.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 110ISO 2039
Tensile Strength 55.0 MPa50mm/min; ISO 527
Elongation at Break 15 %50mm/min; ISO 527
Flexural Strength 75.0 MPa2mm/min; ISO 178
Flexural Modulus 2400 MPa2mm/min; ISO 178
Charpy Impact Unnotched NB4J; ISO 179
Charpy Impact, Notched 13.0 kJ/m²4J; ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C120°C/hr; ISO 75
Vicat Softening Point 102 °C
@Load 5.00 kg
50°C/h; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 200 - 220 °C
Middle Barrel Temperature 230 - 240 °C
Front Barrel Temperature 245 - 260 °C
Nozzle Temperature 240 - 250 °C
Melt Temperature 240 - 260 °C
Mold Temperature 50.0 - 80.0 °C
Drying Temperature 80.0 - 95.0 °C
Dry Time 3.00 - 4.00 hour
Back Pressure 1.00 - 5.00 MPa
Screw Speed 30 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKMSN117 / 280969

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.