MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC CYCOLAC™ INP576 ABS (Europe)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Medium flow SAN pellets. FDA compliant (part use must be at room temperature or below).

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccASTM D792
Density 1.08 g/ccISO 1183
Melt Flow 23 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 78 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 122ASTM D785
Tensile Strength at Break 68.0 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 41.0 MPa5 mm/min; ASTM D638
Elongation at Break 2.2 %5 mm/min; ASTM D638
Elongation at Yield 1.4 %5 mm/min; ASTM D638
Tensile Modulus 3970 MPa5 mm/min; ASTM D638
Flexural Yield Strength 68.0 MPa2 mm/min; ISO 178
 96.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3540 MPa2 mm/min; ISO 178
 3570 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 21.0 J/mASTM D256
 13.0 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 1.00 kJ/m²80*10*4; ISO 180/1A
 1.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 87.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 102 °CRate B/50; ISO 306
 106 °CRate B/120; ISO 306
 
Optical PropertiesOriginal ValueComments
Yellow Index 1.0 %ASTM D1925

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10069 / 243536

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.