MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Gantrade BDO (1,4-butanediol)
Categories: Fluid

Material Notes: Gantrade 1,4-butanediol is a difunctional primary alcohol designed for urethane applications. It has a purity specification of >99.85 % and a moisture content of <150 ppm with a target below 100 ppm of water. The shelf life of 1,4-butanediol is 2 years if stored in the unopened, original containers and kept at ~ 20ºC. BDO is hygroscopic. When opened to the atmosphere, BDO will absorb moisture.

Information provided by Gantrade Corporation.

Key Words: C4H10O2 - HO(CH2-CH2-CH2-CH2)OH
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Molecular Weight 90.12 g/mol
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 0.050mg KOH/g
 
Thermal PropertiesOriginal ValueComments
Melting Point 19.0 - 20.0 °C
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.015 %Moisture by K.F.
 
Descriptive Properties
AppearanceClear, Colorless Liquid
CAS Number110-63-4
Color (APHA)<10
Monocyclic Acetal<0.01GC
Purity>99.85%By GC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGANT960 / 249564

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.