MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Mitsubishi PLA 3D Printing Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Tough, easy to use high grade PLA type of filament, ideal for 3D printing. Slightly modified, the filament retains the typical features of PLA, but makes it tougher and less brittle. Due to a low shrinkage factor, PLA will not deform after cooling. Poly Lactic Acid is an industrial compostable plastic made from renewable natural resources and one of the most popular materials for 3D printing.

Features:

  • Easy to print at low temperature
  • Low warping
  • Industrial compostable
  • Limited smell
  • Tougher and less brittle compared to regular PLA
Colors: PLA is available from stock in 33 bright colors. Other colors on request.

Information provided by Mitsubishi Chemical.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/ccISO 1183
Filament Diameter 1750 µmTolerance: 50 µm, =95% Roundness
 2850 µmTolerance: 100 µm, =95% Roundness
Melt Flow 9.5 g/10 min
@Load 2.16 kg,
Temperature 210 °C
ISO 1133
Storage Temperature 15.0 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 66.0 MPaISO 527
Elongation at Break 2.3 %ISO 527
Elongation at Yield 2.3 %ISO 527
Tensile Modulus 3027 MPa(E); ISO 527
Charpy Impact, Notched 3.40 kJ/m²ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 80.0 - 150 °CISO 11357
Vicat Softening Point 60.0 °CISO 306
Glass Transition Temp, Tg 57.0 °CISO 11357
 
Processing PropertiesOriginal ValueComments
Processing Temperature 195 - 215 °CPrinting Temperature
 
Descriptive Properties
Bed Temp=60°C
Moisture Absorption1968 ppmISO 62

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMITS9836 / 301061

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.