MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Inov Chem Donfoam 901 Water base blend polyols
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: This product is a type of blend polyols with 100% water as blowing agent, which is specially researched for rigid PUF. The characteristics are as follows:
(1) good flowability, Suitable for one-time pouring.
(2) excellent foam mechanical properties
(3) excellent high/low temperature dimensional stability

Information provided by Shandong INOV Polyurethane Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 - 1.10 g/cc
Density 0.0600 - 0.0700 g/ccCore Free density, High pressure machine
 0.0600 - 0.0700 g/ccCore Free density, Manual mixing
 0.0600 - 0.0800 g/ccFoam Density; GB/T6343-2009
Water Absorption <= 3.0 %GB 8810
Viscosity 1800 - 2400 cP
Storage Temperature 10.0 - 25.0 °C
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity <= 0.0320 W/m-KGB 3399
 
Processing PropertiesOriginal ValueComments
Cure Time >= 260 secTack free time, High pressure machine
 >= 300 secTack free time, Manual mixing
Gel Time 2.50 - 3.30 minHigh pressure machine
 3.30 - 4.00 minManual Mixing
Shelf Life 6.00 Month
 
Descriptive Properties
AppearanceLight yellow to brown yellow transparent liquid
Closed-cell rate=95%GB 10799
High temperature-resistance140°C
Hydroxyl value300-400 mgKOH/g
Low temperature-resistance-60°C
Recommended Ratio1:1.0-1.1.20 gPOL/ISO
 1:1.0-1.20 gPOL/ISO
Rise time40-70 secHigh pressure machine
 60-90 secManual Mixing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PINOVCHM035 / 312564

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.