MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ LUX2614G PC (Europe)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Lexan LUX2614G (EXRL0944) is a diffusive, high viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Developed for injection molding LED applications

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183
Water Absorption 0.35 %23°C/sat; ISO 62
Moisture Absorption 0.130 %23°C / 50% RH; ISO 62
Moisture Absorption at Equilibrium 0.58 %
@Temperature 100 °C
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 7.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
cm³/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 70ASTM D785
Hardness, Rockwell R 118ASTM D785
Tensile Strength at Break 65.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 63.0 MPa50 mm/min; ISO 527
Elongation at Break 100 %50 mm/min; ISO 527
Elongation at Yield 6.0 %50 mm/min; ISO 527
Tensile Modulus 2300 MPa1mm/min; ISO 527
Flexural Yield Strength 94.0 MPa2 mm/min; ISO 178
Flexural Modulus 2250 MPa2 mm/min; ISO 178
Izod Impact, Notched 650 J/mASTM D256
Izod Impact, Unnotched NBASTM D4812
Izod Impact, Notched (ISO) 60.0 kJ/m²80*10*3; ISO 180/1A
 11.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*3; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*3 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 63.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 12.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Impact Test 130 JMultiaxial Impact; ISO 6603
Taber Abrasion, mg/1000 Cycles 10CS-17, 1 kg; ASTM D1044
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Dielectric Constant 2.96
@Frequency 1e+6 Hz
ASTM D150
 3.17
@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 15.0 kV/mm
@Thickness 3.20 mm
in air; ASTM D149
Dissipation Factor 0.00090
@Frequency 50.0 - 60.0 Hz
ASTM D150
 0.010
@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index 175 - 250 VUL 746A
Hot Wire Ignition, HWI 15 - 30 secUL 746A
High Amp Arc Ignition, HAI 60 - 120 arcsUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 68.4 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E831
Specific Heat Capacity 1.26 J/g-°CASTM C 351
Thermal Conductivity 0.200 W/m-KASTM C177
Hot Ball Pressure Test 125 °CIEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 123 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
Vicat Softening Point 143 °CRate B/50; ISO 306
 144 °CRate B/120; ISO 306
UL RTI, Electrical 130 °CUL 746B
UL RTI, Mechanical with Impact 125 °CUL 746B
UL RTI, Mechanical without Impact 125 °CUL 746B
Flammability, UL94 V-2
@Thickness 0.750 mm
UL 94
Glow Wire Test 750 °C
@Thickness 0.750 mm
IEC 60695-2-12
 850 °C
@Thickness 1.50 mm
IEC 60695-2-12
 850 °C
@Thickness 1.50 mm
IEC 60695-2-13
 875 °C
@Thickness 0.750 mm
IEC 60695-2-13
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.586ISO 489
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °CHopper Temperature
Nozzle Temperature 270 - 290 °CInjection Molding
Zone 1 260 - 280 °C
Zone 2 270 - 290 °C
Zone 3 280 - 300 °C
Melt Temperature 280 - 300 °C
Mold Temperature 80.0 - 100 °C
Drying Temperature 120 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %
 
Descriptive Properties
UV-light, water exposure/immersionF2UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10505 / 243972

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.