MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Semitron® ESd 490HR Static dissipative PEEK for use in test fixtures. Non-sloughing and low moisture absorption. (ASTM Product Data Sheet)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes:

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.50 g/ccASTM D792
Water Absorption 0.18 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 1.65 %Immersion; ASTM D570(2)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 105ASTM D785
Hardness, Rockwell R 123ASTM D785
Tensile Strength 14000 psiASTM D638
Tensile Strength at 150°C (300°F) 2000 psiASTM D638
Tensile Strength at 65°C (150°F) 12000 psiASTM D638
Elongation at Break 2.3 %ASTM D638
Tensile Modulus 940 ksiASTM D638
Flexural Strength 21000 psiASTM D790
Flexural Modulus 950 ksiASTM D790
Compressive Strength 26000 psi10% Def.; ASTM D695
Compressive Modulus 600000 psiASTM D695
Izod Impact, Notched 1.00 ft-lb/inASTM D256 Type A
Coefficient of Friction, Dynamic 0.20Dry vs. Steel; QTM55007
Limiting Pressure Velocity 17000 psi-ft/min4:1 safety factor; QTM 55007
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1.00e+10 - 1.00e+12 ohmEOS/ESD S11.11
Dielectric Constant 5.33
@Frequency 1e+6 Hz
ASTM D150
Dissipation Factor 0.227
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 28.0 µin/in-°F
@Temperature -40.0 - 149 °C
ASTM E831
Melting Point 644 °FCrystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 475 °FLong Term
Deflection Temperature at 1.8 MPa (264 psi) 500 °FASTM D648
Flammability, UL94 V-0
@Thickness 3.17 mm
Estimated Rating
 
Compliance PropertiesOriginal ValueComments
3A-Dairy No
Canada AG No
FDA No
NSF No
USDA No
USP Class VI No
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Limited
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Alkalies, Weak Limited
Chlorinated Solvents Acceptable
Conductive / Static Dissipative Yes
Continuous Sunlight Acceptable
Hot Water / Steam Acceptable
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable
 
Descriptive Properties
Machinability41-10, 1=Easier to Machine

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Semitron® ESd 480 PEEK, static dissipative, (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Semitron® ESd 520HR (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Semitron® MDS 100 (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Semitron® MP-370 (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Semitron® ESd 225, Extruded, Static Dissipative Acetal (ASTM Product Data Sheet)

P1SM32M / 20124

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.