CALIBRE™ 300EP-22 Series are polycarbonate resins that offer exceptional impact resistance, heat distortion resistance, and optical clarity for injection molding applications. Their high melt flow rate allows complex parts to be easily molded. The CALIBRE™ 300EP-22 Series products are available in 4 additive packages: CALIBRE 300EP: No mold release or UV Stabilizer. CALIBRE 301EP: Mold release. CALIBRE 303EP Mold release and UV stabilizer. Govt and Industry Standards: - CSA (Canadian Standards Association)
- Underwriters Laboratory, Inc (UL)
Applications:- Appliances
- Storage
- Electrical components
- Light diffusers
Information provided by Trinseo. |