MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Danquinsa DANMELTTHANE® PES-680-G Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: DANMELTTHANE® PES-680-G is a saturated Co-polyester-adhesive. It is specially used for the bonding of filters. DANMELTTHANE® PES-680-G distinguishes itself by a high melting point and an optimal melting viscosity for the bonding of filters. Films of DANMELTTHANE® PES-680-G are very flexible and extremely break resistant. When cutting the bonded filter elements, the tools are not being contaminated by the glue line of DANMELTTHANE® PES-680-G.

Application: DANMELTTHANE® PES-680-G makes it possible to do the folding and the joining of filter-web papers before and/or after the impregnation with phenol resin and/or the polymerization. The polymerization temperature is supposed to be between 170 and 180 °C. DANMELTTHANE® PES-680-G is qualified for the filter bonding of automobile-, air-, industrial-, household-, protection-, dirt-, dust- and medical filters.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/cc
Brookfield Viscosity 25000 - 35000 cP
@Temperature 232 °C
RVT
 
Thermal PropertiesOriginal ValueComments
Melting Point 210 - 220 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 220 - 240 °C
Shelf Life 6.00 Month
 
Descriptive Properties
AspectGranules
Open time<10 sec
Polymerization temperature<180°Cduring the at process of filter production
TypeSaturated thermoplastic polyester

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDANQ125 / 294545

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.