MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Hostaform® S 9363 XAP² ™ POM, Impact Modified
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Impact Modified

Material Notes: Hostaform« acetal copolymer grade S 9363 XAP2 Ö is an impact modified grade for demanding applications. Hostaform« S 9363 XAP2 Ö provides good impact strength while improving modulus and weld line strength over standard impact modified grades such as Hostaform« S 9063, and also exhibits exceptional low emission performance meeting or exceeding the requirements of many automotive markets.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.38 g/ccISO 1183
Water Absorption at Saturation 0.80 %ISO 62
Linear Mold Shrinkage, Flow 0.018 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.016 cm/cmISO 294-4
Melt Flow 5.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
[cm3/10min]; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 50.0 MPa50mm/min; ISO 527-2/1A
Elongation at Yield 12 %50mm/min; ISO 527-2/1A
Tensile Modulus 2000 MPa50mm/min; ISO 527-2/1A
Flexural Modulus 2000 MPaISO 178
Charpy Impact Unnotched NBISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 13.0 kJ/m²ISO 179/1eA
 8.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 110 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 110 µm/m-°CISO 11359-2
Melting Point 166 °C10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 148 °CISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °CISO 75-1, -2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 70.0 °Ccavity
Zone 1 170 - 180 °C
Zone 2 180 - 190 °C
Zone 3 180 - 190 °C
Zone 4 180 - 200 °C
Die Temperature 180 - 200 °C
Melt Temperature 180 - 200 °C
Drying Temperature 80.0 - 100 °C
Dry Time 3.00 hour
Injection Pressure 60.0 - 120 MPa
Hold Pressure 60.0 - 120 MPa
Back Pressure <= 2.00 MPa
 
Descriptive Properties
Injection moldingYes
Injection speedslow
Processing conditions acc. ISO9988-2
Profile extrusionYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Hostaform® S 9363 POM, Impact Modified
Celanese Celcon® LW90-S2 POM, Tribological
Celanese Hostaform® S 9364 XAP² ™ POM, Impact Modified
Celanese Hostaform® S 9362 XAP² ™ POM, Impact Modified
Celanese Hostaform® S 9362 POM, Impact Modified

PHCQ422 / 178877

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.