MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Zytel® FR70G25V0 BK369 PA66-GF25FR(17)  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: 25% Glass Reinforced, Flame Retardant, Polyamide 66

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.53 g/ccDAM; ISO 1183
Melt Density 1.35 g/cc
@Temperature >=260 °C
Water Absorption 3.4 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Moisture Absorption 0.900 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cmDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.010 cm/cmDAM; ISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 110 MPa50% RH; ISO 527-1/-2
 130 MPaDAM; ISO 527-1/-2
Elongation at Break 2.4 %DAM; ISO 527-1/-2
 3.4 %50% RH; ISO 527-1/-2
Tensile Modulus 6500 MPa50% RH; ISO 527-1/-2
 9000 MPaDAM; ISO 527-1/-2
Poissons Ratio 0.34DAM; ISO 527-1/-2
 0.3550%RH; ISO 527-1/-2
Charpy Impact Unnotched 50.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 9.50 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 11.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 26.0 µm/m-°CDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 83.0 µm/m-°CDAM; ISO 11359-1/-2
Specific Heat Capacity 1.91 J/g-°C
@Temperature >=260 °C
Melt
Thermal Conductivity 0.220 W/m-K
@Temperature >=260 °C
Melt
Melting Point 260 °C10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 243 °CDAM; ISO 75-1/-2
Vicat Softening Point 235 °C50°C/h, 50N; ISO 306
Flammability, UL94 V-0
@Thickness 0.830 mm
DAM; IEC 60695-11-10
 V-0
@Thickness 1.50 mm
DAM; IEC 60695-11-10
 5VA
@Thickness 1.50 mm
DAM; IEC 60695-11-20
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 - 300 °CInjection
 290 °CInjection Optimum
Mold Temperature 70.0 - 120 °CInjection
 100 °CInjection Optimum
Ejection Temperature 210 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 2.00 - 4.00 hourDehumidified Dryer; Injection
Moisture Content 0.20 %Injection
Hold Pressure 50.0 - 100 MPaInjection
 
Descriptive Properties
AdditivesRelease agent
Delivery formPellets
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
Hold pressure time (s/mm)3Injection
Max. screw tangential speed (m/s)0.2Injection
Part Marking CodePA66-GF25FR(17)ISO 11469
ProcessingInjection Molding
Regional AvailabilityEurope
 Near East/Africa
Resin IdentificationPA66-GF25FR(17)ISO 1043

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® FR70G25V0 NC010 PA66-GF25FR(17)
Envalior Novamid® 3010GN30 NAT PA66-GF30 FR(17)
Trinseo Plexiglas® V052 Acrylic
Trinseo Plexiglas® V052i Acrylic
Celanese Zytel® FR50 BK505 PA66-GF25FR(17)

PDSX5424 / 198064

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.