MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco HDAX® SAE 40 LFG Gas Engine Oil
Categories: Fluid; Lubricant

Material Notes: Features

Chevron HDAX LFG Gas Engine Oil is a premium quality, medium ash, dispersant/detergent type gas engine oil formulated especially for landfill gas and sour gas application.

It is formulated with ISOSYN™ base stocks and an additive package containing ashless dispersant, oxidation inhibitors, metallic detergents, a metallic antiwear additive, and a special combination of inhibitors to protect engines from the corrosive combustion byproducts encountered when landfill gas and sour gas are used.

Chevron HDAX LFG Gas Engine Oil provides outstanding corrosion resistance in landfill gas and sour gas applications, even when intermittent operation results in the formation of significant levels of acidic condensate. At 0.7 wt% ash, Chevron HDAX LFG Gas Engine Oil gives this performance with out the higher levels of combustion chamber deposits associated with other products used in this application.

It also provides an extra measure of valve protection for those four-stroke engines where medium ash oils are preferred (e.g., Superior and Waukesha).

Chevron HDAX LFG Gas Engine Oil provides excellent piston deposit control to minimize the possibility of ring sticking.

Applications

Chevron HDAX LFG Gas Engine Oil is especially recommended for four-cycle engines fueled by landfill gas containing elevated levels of Chloro-Fluoro-Carbons (CFCs) and sour gas applications where corrosive wear is a special concern. The low phosphorous level (270 ppm) of Chevron HDAX LFG Gas Engine Oil makes it compatible with Engelhard NSCR emissions catalysts.

Key Words: CPS Number: 232325; MSDS Number: 11768
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 27.5 °
Viscosity Measurement 105Viscosity Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 145 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 15.1 cStASTM D445
Ash 0.71 %Sulfated Ash wt%
 
Chemical PropertiesOriginal ValueComments
Total Base Number 6.0ASTM D2896
 
Thermal PropertiesOriginal ValueComments
Pour Point -18.0 °CASTM D97
Flash Point 232 °CASTM D92
 
Component Elements PropertiesOriginal ValueComments
Phosphorus, P 0.027 %
Zinc, Zn 0.031 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCHEV059 / 74674

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.