MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ganpati Exim CTP (PVI)
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Molecular Formula: C14H15O2NS

Properties : It is white or yellow crystalline. It can be dissolved in acetone, benzene, toluene, ethyl ether and ethyl acetate as well as warm carbon tetra chloride, ethyl alcohol and heptane. It also can be slightly dissolved in gasoline, but not in kerosene and water.

Application : The product may be used in natural rubber and synthetic rubber. It may protect effectively the rubber material from scorching during Processing, So that to make it possible for extruder and calendar to be running at a high temperature and high speed and improve the production capacity of vulcanizer. The product also can improve the storage stabilization of the rubber material, protect natural vulcanization during storage. It has reclaimation function for rubber material, which bearing high heating or with dangers of scorching.

Information provided by Ganpati Exim PVT. LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Ash <= 0.10 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 89.0 - 94.0 °C
 
Descriptive Properties
AppearanceWhite or light yellow powered crystal
Content<0.5%Insoluble matter in toluene
 <96%Available composition content
Heating Loss0.005

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGANPATI084 / 317368

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.