MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC SABIC® SSBR 3323H Synthetic Rubber (Global)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: SABIC® SSBR 3323H is a medium vinyl, high styrene solution polymerized styrene butadiene rubber. It is manufactured by anionic copolymerization using Lithium catalyst. SABIC® SSBR 3323H is an oil extended polymer with 37.5 Phr low-PCA oil and stabilized with a non-staining anti-oxidant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles 0.75 %ASTM D5668
Mooney Viscosity 60ML 1+4 @100 °C; ASTM D1646
 
Chemical PropertiesOriginal ValueComments
Styrene Content 33 %SABIC method
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -35.0 °COnset Tg of contained polymer; SABIC method
 
Descriptive Properties
AppearanceTan to dark brown VisualVisual
Oil Content27.3 %ASTM D5774
Vinyl Content(On polymer)23 %SABIC method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI11620 / 245087

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.