MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Vistac® ISO 220 Way Oil
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Way Oils Vistac provide extreme pressure and antiwear protection and have stringiness and oiliness characteristics. As indicated by part of the name, Vistac, these lubricants have an unusual adhesive or tacky quality.

Chevron Way Oils Vistac reduce leakage and adhere to metal surfaces providing a tenacious lubricant film. Chevron Way Oils Vistac are formulated to meet the critical lubrication demands for the slides and ways of machine tools.

Their inherent low coefficient of static friction eliminates stick-slip or jerky motion of sliding parts on machine tools which increase operating efficiency of the tools and smoother overall operation.

Due to their adhesiveness, these oils form a tenacious film which resists being wiped away by the slowly moving parallel surfaces of the way or being washed away by cutting fluids.

Their antiwear and extreme pressure properties protect the sliding surfaces.

These oils also protect cast iron and bronze surfaces from rust and corrosion, and are resistant to oxidation to provide long lubricant life.

Applications

Chevron Way Oils Vistac have proven excellence in the lubrication of ways in many types of machine tools, e.g., lathes, planers, shapers, drilling and tapping machines, etc., including those operating at high loads. These oils provide many performance characteristics that lend themselves well to lubrication of enclosed gears and all types of industrial plain and antifriction bearings.

Their tacky quality makes these oils suitable for oncethrough applications, e.g., lubrication of chain drives. If contamination with soluble oils is a problem, Chevron Way Oils Vistac® D is recommended. Chevron Way Oils Vistac meet the requirements of:

  • Cincinnati Machine P-47 (ISO 68), P-50 (ISO 220) specifications for way lubricants
  • Hardinge Groove Print Stain Test (ISO 68)
Chevron Way Oils Vistac are registered with NSF and are acceptable as a lubricant where there is no possibility of food contact (H2) in and around food processing areas. The NSF Nonfood Compounds Registration Program is a continuation of the USDA product approval and listing program, which is based on meeting regulatory requirements of appropriate use, ingredient review and labeling verification.

Key Words: CPS Number: 232512; MSDS Number: 7459
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 25.7 °
Viscosity Measurement 60Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 1121 SUS
Saybolt Viscosity at 210°F 79.9 SUS
Kinematic Viscosity at 40°C (104°F) 209 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 15 cStASTM D445
 
Thermal PropertiesOriginal ValueComments
Pour Point -15.0 °CASTM D97
Flash Point 234 °CASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCHEV381 / 74996

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.