MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BYK Optiflo® M2600 Nonionic Associative Thickener
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: OPTIFLO M2600 is a solution of a nonionic hydrophobe modified polymer. OPTIFLO M2600 is suitable rheology modifier for acrylic, styrene-acrylic, EVA, and vinyl acrylic latex systems. The solution consists of water and glycol ether DB.

Application:

  • Architectural coatings (especially in acrylic based resin systems)
  • Industrial coatings (especially in acrylic based resin systems)
  • Particularly suited for larger particle size acrylics, vinyl acrylics, VAE, VaVEOVa, and styreneacrylic systems.

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/cc
Solids Content 24.2 %Volume
 25 %Weight
pH 7.0 - 8.0
Viscosity 1000 - 3000 cP
 
Descriptive Properties
Color/FormClear solution
Solvent81/19water/glycol ether DB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BYK Optiflo® H7500 VF Polymer
BYK Optiflo® H6500 VF (formerly RXL-7255) Polymer
BYK Optiflo® H600 VF Polymer
BYK Optiflo® H600 Polymer
BYK Optiflo® H400 Polymer

PBYK098 / 185095

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.