MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Makroblend® DP 2-7655 MBS162 Polycarbonate + PET, Mineral Filled Impact Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes:
  • Developmental product
  • (PC+PET)-blends
  • impact modified
  • Injection molding grade 10% mineral filled

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Modulus 3100 MPaISO 527-1/-2
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 60.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 60.0 µm/m-°CISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 128 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 110 °CISO 75-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 - 280 °C
 270 °CInjection Molding; ISO 294
Mold Temperature 60.0 - 80.0 °C
 70.0 °CInjection Molding; ISO 10724
Injection Velocity 200 mm/secISO 294
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Near East/Africa
 North America
 South and Central America
FeatureRelease agent
FormPellets
ProcessInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makroblend® DP 2-7655 Polycarbonate + PET, Mineral Filled Impact Grade
Covestro Makroblend® UT305 PC/PET Blend
Covestro Makroblend® EL 703 Polycarbonate + Polyester-based Blend, Impact Modified, Flame-Retardant, UV Stabilized
Covestro Makroblend® DP 7645 Polycarbonate + PET, Impact Grade
Covestro Makroblend® DP 7665 Polycarbonate + PET, Mineral Filled Impact Grade

PB09833 / 92673

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.