MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Toyobo Celstran® PP-GF40-0455 Soul 4PK Black PP, 40% Long Glass Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Glass Fiber Filler

Material Notes: Product Description: Material code according to ISO 1043-1: PP UV-stabilized, reinforced with 40% long glass fibers, low emission. The fibers are chemically coupled to the polypropylene matrix. The pellets are cylindrical and normally as well as the embedded fibers 10 mm long. Parts molded of Celstran have outstanding mechanical properties such as high strength and stiffness combined with high heat deflection. The notched impact strength is increased at elevated and low temperatures due to the fiber skeleton build in the parts. The long fibber reinforcement reduces creep significantly. The very isotropic shrinkage in the molded parts minimizes the warpage. Complex parts can be manufactured with high reproducibility by injection molding. Application field: Functional/structural parts for automotive.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Filler/Reinforcement: Glass Fiber

Features: Good Heat Resistance; Low Emissions; UV Resistant

Use: Coating Applications; Profiles; Sheet

Form: Pellets

Processing Method: Coating; Injection Molding; Resin Transfer Molding; Extrusion; Profile Extrusion; Sheet Extrusion

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccISO 1183
Maximum Moisture Content 0.20
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 17400 psiISO 527-2/5
Elongation at Break 2.0 %ISO 527-2/5
Tensile Modulus 1.31e+6 psiISO 527-1
Flexural Strength 17400 psi
@Temperature 80.0 °C
ISO 178
 29000 psi
@Temperature 22.8 °C
ISO 178
Flexural Modulus 885000 psi
@Temperature 80.0 °C
ISO 178
 1.22e+6 psi
@Temperature 22.8 °C
ISO 178
Poissons Ratio 0.35ISO 527
Charpy Impact Unnotched 26.0 ft-lb/in²
@Temperature -30.0 °C
ISO 179/1eU
 29.0 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eU
Charpy Impact, Notched 14.0 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eA
 15.0 ft-lb/in²
@Temperature -30.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 329 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 324 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 320 °FUnannealed; ISO 75-2/A
Deflection Temperature at 8.0 MPa 275 °FUnannealed; ISO 75-2/C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 446 - 518 °FHot Runner
Feed Temperature 68.0 - 122 °FInjection
Rear Barrel Temperature 410 - 446 °F
Middle Barrel Temperature 428 - 464 °F
Front Barrel Temperature 446 - 482 °F
Nozzle Temperature 446 - 482 °F
Zone 4 446 - 482 °FInjection
Melt Temperature 446 - 482 °F
Mold Temperature 86.0 - 158 °F
Drying Temperature 194 - 212 °F
Dry Time 2.00 hour
Back Pressure <= 435 psi
Screw Speed 25 rpm
@Thickness 76.2 mm
 35 rpm
@Thickness 55.9 mm
 50 rpm
@Thickness 40.6 mm
 
Descriptive Properties
Burn0.94 in/mm0.0394, FMVSS 302, ISO 3795
Emission of Organic Compounds30 µgC/gVDA 277
Odor3.5VDA 270

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHCQ6256 / 310949

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.