MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dover Chemical DOVERGUARD 68 Halogenated Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Doverguard 68 is a flame retardant containing both aromatic and aliphatic bromine. Doverguard 68 melts during process to give good dispersion and good thermal stability

Information provided by DoverChem

Key Words: CAS# 21850-44-2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.20 g/cc
@Temperature 25.0 °C
Bulk Density 0.760 g/cc
@Temperature 25.0 °C
Loose
 1.10 g/cc
@Temperature 25.0 °C
Packed
Solubility in Water <= 0.10 %
Solubility 1000 ppmMethanol
 70000 ppmMethyl Ethyl Ketone
 100000 ppmStyrene
 240000 ppmToluene
 500000 ppmMethylene Chloride
 
Thermal PropertiesOriginal ValueComments
Melting Point 106 - 120 °C
 
Descriptive Properties
AppearanceOff-White Powder
Bromine, %68
Loss on Drying, %1010mg @10°C/minute under N2
 510mg @10°C/minute under N2
 5010mg @10°C/minute under N2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WDOVER020 / 217639

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.