MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Astryn BR33GC Polypropylene Copolymer, Mineral Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes:
Key Features: conventional melt flow, high modulus, UV-stabilized, mineral-filled polypropylene copolymer, high rigidity, high impact strength, good dimensional stability, low fogging

Applications: knee bolsters, map pocket bins, glove box doors

Description: Astryn BR33GC conventional melt flow, UV-stabilized, precolored, mineral-filled polypropylene copolymer has an excellent balance of rigidity, impact strength and dimensional stability. It was designed for a variety of automotive interior trim applications.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccASTM D792B
Linear Mold Shrinkage 0.011 cm/cmISO Method 2577
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65ISO 868
Tensile Strength, Yield 21.0 MPaISO Method R527
Elongation at Yield 5.0 %ISO Method R527
Flexural Modulus 1.80 GPaISO Method 178
Izod Impact Resistance 0.170 J/cm²
@Temperature 23.0 °C
ISO 180
 
Thermal PropertiesOriginal ValueComments
CTE, linear 48.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °CISO Method 75

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Moplen HP550J Polypropylene Homopolymer
LyondellBasell Hostacom™ GP622 Polypropylene Homopolymer
LyondellBasell Astryn BB73F Polypropylene Copolymer, Mineral Filled
LyondellBasell Astryn BB725GC Polypropylene Copolymer, Mineral Filled
LyondellBasell Astryn BA45H Polypropylene Copolymer, Flame Retardant

PMO390 / 53619

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.