MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Covestro Baytec® SPR-092A Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Baytec SPR-092A is a two-component, 100%-solids spray system with a Shore A hardness of 92*.

Properties / Applications: Baytec SPR-092A is a two-component, 100%-solids spray system with a Shore A hardness of 92*. The isocyanate component is a modified diphenylmethane diisocyanate (MDI) prepolymer, and the polyol component is a polyether polyol blend. The system has added UV stabilizers and is used in spray applications to improve the corrosion, weather, and abrasion resistance of various surfaces. In-mold application is also possible. Typical applications include protective layers for pipes, tanks, fabrics, wood, flexible foams, and other industrial surfaces. The system can be pigmented to almost any color. As with any product, use of the Baytec SPR-092A system in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccPolyol
 1.083 g/ccASTM D792
 1.09 g/ccIsocyanate
Water Absorption 1.5 %
@Time 2.59e+6 sec
Viscosity 1500 cPPolyol
 2500 cPIsocyanate
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 92ASTM D2240
Tensile Strength at Break 15.2 - 15.9 MPaASTM D412
Elongation at Break 490 - 580 %ASTM D412
Tear Strength 110 - 130 pliSplit Tear; ASTM D1938
 340 - 410 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 150
@Load 1.00 kg
H-18; ASTM D4060
 
Thermal PropertiesOriginal ValueComments
Flash Point 179 °CPolyol
 216 °CIsocyanate
 
Processing PropertiesOriginal ValueComments
Gel Time 0.200 - 0.250 min
 
Descriptive Properties
AppearanceWhite liquidPolyol
 Yellowish liquidIsocyanate
Content9.8%NCO, Isocyanate
Hydroxyl number[mg KOH/g], Polyol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Baytec® SPR-092A Black Polyurethane
Covestro Baytec® RTC-092A Polyurethane
Covestro Baytec® RTC V85 Component A Polyurethane
Covestro Bayflex® MP-10000 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
Covestro Bayflex® LSR 10 Elastomer

PCOVEST0264 / 202047

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.