MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Celanese Vandar® 2122 PBT, 10% Mineral Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Mineral Filled

Material Notes: Vandar 2122 is a polyester alloy which contains 10% mineral filler. It offers exceptional toughness and practical impact strength. This resin offers Class A paintable finish with excellent dimensional stability.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccASTM D792
Density 1.30 g/ccISO 1183
Water Absorption 0.10 %
@Temperature 22.8 °C
24hr immersion; ASTM D570
Linear Mold Shrinkage, Flow 0.013 - 0.015 cm/cmASTM D955
 0.013 - 0.015 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.013 - 0.015 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 104ISO 2039-2
Tensile Strength, Yield 6400 psiASTM D638
Tensile Stress at Strain 30.0 MPa
@Strain 50 %
ISO 527-2/1A
Elongation at Break >= 50 %
 80 %ASTM D638
Flexural Strength 55.0 MPaISO 178
 9200 psiASTM D790
Flexural Modulus 1900 MPaISO 178
 325000 psiASTM D790
Izod Impact, Notched 3.00 ft-lb/inASTM D256
 1.00 ft-lb/in
@Temperature -28.9 °C
ASTM D256
Izod Impact, Notched (ISO) 15.0 kJ/m²ISO 180/1A
 
Thermal PropertiesOriginal ValueComments
Melting Point 225 °C10°C/min; ISO 11357-1,-2,-3
 437 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 128 °CISO 75-1, -2
 270 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 53.0 °CISO 75-1, -2
 120 °FASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 65.0 - 96.0 °Ccavity
 250 - 260 °Chot runner
Feed Temperature 230 - 240 °C
Zone 1 230 - 240 °C
Zone 2 235 - 250 °C
Zone 3 235 - 250 °C
Zone 4 240 - 260 °C
Die Temperature 240 - 260 °C
Melt Temperature 235 - 260 °C
 260 °CISO 294
Mold Temperature 82.0 °CISO 294
Injection Velocity 300 mm/secISO 294
Drying Temperature 120 - 130 °C
Dry Time 4.00 hour
Moisture Content <= 0.020 %
Hold Pressure 86.0 MPaISO 294
 
Descriptive Properties
Injection moldingYes
Injection speedmedium-fast
Processing conditions acc. ISO7792-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Vandar® 6000 PBT, Unfilled
Celanese Vandar® 4602ZHR PBT, Unfilled
Celanese Vandar® 4602Z PBT, Unfilled
Celanese Vandar® 2500 PBT, Unfilled
Celanese Vandar® 2100UV PBT, Impact Modified

PHCQ475 / 178930

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.