MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polymer Resources ABS-FR-[color]-UV Flame Retardant ABS, UV-stabilized
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant

Material Notes: Flame Retardant Acrylonitrile Butadiene Styrene, UV-stabilized

Features: • Flame Retardant • Self Extinguishing • Good UV Resistance
Process: Injection Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.

Information provided by Polymer Resources Corporation.

Key Words: UL E113219
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cmASTM D955
Melt Flow 4.0 - 16 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 100ASTM D785
Tensile Strength at Break 5500 psiASTM D638
Tensile Strength, Yield 5900 psiASTM D638
Elongation at Break 10 %ASTM D638
Elongation at Yield 2.2 %ASTM D638
Tensile Modulus 330000 psiASTM D638
Flexural Strength 9000 psiASTM D790
Flexural Modulus 345 ksiASTM D790
Izod Impact, Notched 4.00 ft-lb/in
@Temperature 22.8 °C
ASTM D256
Izod Impact, Notched (ISO) 3.00 ft-lb/in²
@Temperature -30.0 °C
ISO 180/1A
 9.00 ft-lb/in²
@Temperature 22.8 °C
ISO 180/1A
Charpy Impact, Notched 9.00 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eA
Gardner Impact 150 in-lbASTM D3029
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 190 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 180 °FASTM D648
Vicat Softening Point 195 °F120°C/h, 50 N; ASTM D1525
UL RTI, Electrical 140 °F
@Thickness 1.50 mm
UL 746
 140 °F
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical with Impact 140 °F
@Thickness 1.50 mm
UL 746
 140 °F
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical without Impact 140 °F
@Thickness 1.50 mm
UL 746
 140 °F
@Thickness 3.00 mm
UL 746
Flammability, UL94 V-0
@Thickness 1.50 mm
 V-0 - 5VA
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 340 - 360 °F
Middle Barrel Temperature 390 - 410 °F
Front Barrel Temperature 410 - 430 °F
Melt Temperature 400 - 450 °F
Mold Temperature 120 - 160 °F
Drying Temperature 180 - 200 °F
Dry Time 2.00 - 4.00 hour
Vent Depth 0.00100 in
 
Descriptive Properties
Outdoor Suitabilityf2UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polymer Resources ABS-FR Flame Retardant ABS
Chi Mei Polylac® PA-764 ABS - Flame Retardant
Chi Mei Polylac® PA-764B ABS - Flame Retardant
Chi Mei Polylac® PA-763 ABS - Flame Retardant
Avient Edgetek® CY-1000 UV FR V0 Acrylonitrile Butadiene Styrene + PC (ABS+PC)

PPOLYQ002 / 160514

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.