MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Pyro-Stack Modules Kaowool SZr/Cerachem Blanket Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Pyro-Stack modules comprise strips of high quality spunfibre blanket, compressed and banded with plastic strips and including two stainless steel tubes mounted transversely through the strips remote from the hot face. They can be anchored to the furnace casing in any one of four standard versions, Y, M, T and Eye-bolt.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.28 g/cc
@Temperature 23.0 °C
50% RH
 1.60 g/cc
@Temperature 23.0 °C
50% RH
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.13 J/g-°C
@Temperature 1090 °C
Thermal Conductivity 0.110 W/m-K
@Temperature 400 °C
at 160kg/m3
 0.120 W/m-K
@Temperature 400 °C
at 128kg/m3
 0.180 W/m-K
@Temperature 600 °C
at 160kg/m3
 0.190 W/m-K
@Temperature 600 °C
at 128kg/m3
 0.250 W/m-K
@Temperature 800 °C
at 160kg/m3
 0.280 W/m-K
@Temperature 800 °C
at 128kg/m3
 0.340 W/m-K
@Temperature 1000 °C
at 160kg/m3
 0.380 W/m-K
@Temperature 1000 °C
at 128kg/m3
Maximum Service Temperature, Air 1425 °CContinuous Use
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMORF7071 / 203370

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.