Product Description: LD 150 series are LDPE grades, offering good blend mechanical properties and stiffness. Several additive packages are available according to the required surface properties. Availability: Africa & Middle East, Asia Pacific and Europe Additive: - Antiblock: No
- Slip: No
- Thermal Stabilizer: Yes
Applications: - Agricultural Film
- Blend Partner
- Co-Extrusion Films
- Collation Shrink
- Form Fill and Seal Packaging
- Freezer Film
- Lamination Film
- Medium Duty Shrink Film
- Shoppers
Information provided by ExxonMobil |