MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Solvay MTM® 56 series Epoxy Resin
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: MTM56 series prepregs are based on 120°C (248°F) curing toughened, epoxy matrix resins that have been specifically developed for rapid cure of components. MTM56 series prepregs exhibit excellent toughness and, after a suitable post-cure, can be used at temperatures up to 100°C (212°F).

Features & Benefits:

  • Versatile processing: autoclave, oven vacuum bag and press molding
  • Rapid cure: 10 minutes at 120°C (248°F)
  • 30 days out life at 21°C (70°F)
  • 12 months storage at -18°C(0°F)
  • Available in ZPREG selective impregnation format
  • Good tack and drape
  • Good impact resistance
  • 100°C (212°F) end use temperature
  • 5 hours at 80°C (176°F) minimum cure
Product variants:
MTM56B: Black pigmented woven prepreg
MTM56FR: Flame-retarded, black pigmented woven prepreg
MTM56FRB: Flame-retarded, black pigmented woven prepreg
MTM56FRNY: Flame-retarded, yellow pigmented woven prepreg
MTM56-1: Unidirectional prepreg
MTM56-1B: Black pigmented unidirectional prepreg

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccCured resin, 10 mins at 120°C
Storage Temperature -18.0 °C
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength >= 287000 psi0°, Note 1
Flexural Modulus 132 GPa0°, Note 1; CRAG 200
Shear Strength 13200 psi0° Interlaminar, Note 1; ASTM D2344
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 100 °C
Glass Transition Temp, Tg 100 °CDMA E' onset Tg, 10 mins at 120°C
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 hour
@Temperature 80.0 °C
Shelf Life 12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexPly® F593 Epoxy Resin
Overview of materials for Epoxy/Carbon Fiber Composite
Master Bond EP21SC-1 Two Component Epoxy Resin System
Master Bond EP21LSCL-1 Two Component, Room Temperature Curing Epoxy Resin
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 52%/G1177 Glass/Carbon Fiber

PCYTED149 / 180451

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.