MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Inov Chem DDPU - 301 Polyurethane grouting material
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE

Material Notes: Introduction: DDPU - 301 is a two-component hydrophobic polyurethane grouting material, designed for rescue and relief . The material have a very short reaction time and quickly transform from a liquid to their final foam form. This material can not only waterproof plugging, but also has a certain reinforcement and stabilization effect. It has been widely used in subway tunnels, water conservancy and hydropower, underground garage, sewer and other fields of waterproof leakage-plugging.

Features:

  • Rapid react with water, fast foaming expand and cure. The reaction time can be adjusted according to the amount of component A, generally can be controlled to cure in tens of seconds to minutes
  • Chemical stability is excellent
  • High strength. The compressive strength can go over 20MPa within a few hours when molding under airtight conditions
  • With large infiltration radius and solidification volume ratio, rapid chemical reaction. When the material encounter water, great expansion pressure will be generated to push the slurry deep into the crack to form a tough consolidation.
Application:
  • Seam sealing and waterproof anticorrosive coating of pool, water tower, basement, air raid shelter and other buildings
  • Anticorrosion of metal and concrete pipelines and steel structures
  • Dust treatment ,underground tunnel or building foundation reinforcement
  • Sealing and strengthening of deformation seams, construction joints and structural cracks in construction projects
  • Sealing leakage and strengthening ports, wharves, piers, dams and hydropower stations
  • Wall protection and leak plugging in geological drilling, selective water plugging in oil exploitation, and water stop-gushing in the mine, etc.

Information provided by Shandong INOV Polyurethane Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 - 1.10 g/ccA component CAT.
 1.05 - 1.30 g/ccCuring Performance
 1.15 - 1.25 g/ccB component PU
Solids Content >= 82 %Setting time
Volatiles <= 10 %B component PU
Viscosity <= 60 cPA component CAT.
 <= 600 cPB component PU
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength >= 20.0 MPaSetting time
 
Processing PropertiesOriginal ValueComments
Cure Time <= 90.0 secCuring Performance, Setting time
 
Descriptive Properties
AppearanceLight yellow transparent liquidA component CAT.
 Tan transparent liquidB component PU
Foaming rate=2000%Curing performance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PINOVCHM041 / 312570

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.