MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Nouryon DMZn SSG Dimethylzinc
Categories: Other Engineering Material

Material Notes: DMZn SSG is a zinc precursor (Select Semiconductor Grade) for the deposition of compound semiconductors.

CAS number: 544-97-8

EINECS/ELINCS No.: 208-884-14

Applications: DMZn SSG is used as a high quality zinc precursor for the deposition of compound semiconductors which are used in applications such as light emitting diodes, laser diodes and high efficiency solar cells. Containers are fabricated from stainless steel with an electropolished internal finish and are equipped with dip tube for top discharge and diaphragm valves. The diaphragm valves are equipped with metal gasket face seal connections

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.313 g/cc
Viscosity 0.30 cP
@Temperature 30.0 °C
Molecular Weight 95.5 g/mol
Vapor Pressure 0.0410 bar
@Temperature 20.0 °C
283.15 K
 0.260 bar
@Temperature 10.0 °C
283.15 K
 
Thermal PropertiesOriginal ValueComments
Melting Point -29.0 °C
Boiling Point 44.0 °C
 
Descriptive Properties
AppearanceClear, colorless liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY487 / 286010

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.