MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco L Metal Protective Oil L
Categories: Fluid; Lubricant

Material Notes: Texaco Metal Protective Oil L delivers value through:
  • Excellent short-term rust protection — After evaporation of the solvent, a highly protective, nondrying oil film remains which provides a higher level of protection against corrosion than lower viscosity products. The corrosion inhibitors in the oil resist chemical attack by water, other fluids and particulate matter.
  • Minimum drippage — Viscosity of the oil is low enough to enable ready drain-off of excess oil. High volatility of the solvent ensures rapid evaporation, minimizing post-application dripping.
  • Easy removal — Oil film is readily soluble in petroleum solvent or kerosene to enable easy removal when required.

Texaco Metal Protective Oil L is a higher viscosity, rust protective oil designed for the temporary rust protection of steel in covered storage or packaged shipment.

It contains corrosion inhibitors and is diluted with a petroleum solvent for ease of application.

Texaco Metal Protective Oil L is recommended for:

  • Use as temporary protection of plain and galvanized steel sheet, coils, bars, rods and tubes during undercover storage, protected shipment or interprocess handling
      Protection against yellow-line stain that tends to form on stacked sheets or coiled strip; white rust on galvanized steel; red rust

    May be applied by brush, roller, dip, or spray.

    Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

    CPS Number: 221052; MSDS Number: 10690

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 27.1 °
Saybolt Viscosity at 100°F 92 SUS
Kinematic Viscosity at 40°C (104°F) 17 cSt
 
Thermal PropertiesOriginal ValueComments
Pour Point -23.0 °C
Flash Point 88.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Commercial Steel (CS Type B), Standard Grade
ASTM A525 Galvanized Steel
Aluminum 5052-H32
Tokuyama Shapal™ SH-15 Sintered Aluminum Nitride
ASTM A591 Zinc Coated Steel, Drawing

WTEXA108 / 76987

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.