Ethylene based plastomer produced using ExxonMobil Chemical Exxpol technology, exhibiting both plastic and elastomeric properties. Designed for modification of both polypropylenes and polyethylenes in applications such as injection molding, extrusion blow molding, blown and cast film, and profile extrusion. Supplied with low level antioxidant for process stabilization. Information provided by ExxonMobil Chemical |