MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC GELOY™ CR7500 ASA (Europe)
Categories: Polymer; Thermoplastic; ASA Polymer

Material Notes: ASA, excellent weatherable, injection molding

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccASTM D792
Density 1.07 g/ccISO 1183
Water Absorption 0.50 %23°C/sat; ISO 62
Moisture Absorption 0.200 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 6.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
cm³/10 min; ISO 1133
 6.3 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 10 g/10 min
@Load 5.00 kg,
Temperature 260 °C
cm³/10 min; ISO 1133
 11 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 33.0 MPa5 mm/min; ASTM D638
 35.0 MPa5 mm/min; ISO 527
Tensile Strength, Yield 40.0 MPa5 mm/min; ASTM D638
 43.0 MPa5 mm/min; ISO 527
Elongation at Break 19 %5 mm/min; ISO 527
 60 %5 mm/min; ASTM D638
Elongation at Yield 3.3 %5 mm/min; ISO 527
 3.6 %5 mm/min; ASTM D638
Tensile Modulus 1970 MPa5 mm/min; ASTM D638
 2040 MPa1mm/min; ISO 527
Flexural Yield Strength 64.0 MPa2 mm/min; ISO 178
 68.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2060 MPa2 mm/min; ISO 178
 2170 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 400 J/mASTM D256
 60.0 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 15.0 kJ/m²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 14.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 30.0 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 84.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 84.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 95.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 95.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Hot Ball Pressure Test 98.0 °CIEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
 89.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 90.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 98.0 °CRate B/50; ASTM D1525
 102 °CRate B/50; ISO 306
 105 °CRate B/120; ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 235 - 255 °CInjection Molding
Zone 1 230 - 250 °C
Zone 2 235 - 255 °C
Zone 3 245 - 260 °C
Melt Temperature 255 - 270 °C
Mold Temperature 60.0 - 85.0 °C
Drying Temperature 85.0 - 95.0 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Moisture Content 0.040 %
Back Pressure 0.300 - 1.00 MPa
Shot Size 40 - 80 %
Vent Depth 0.00380 - 0.00760 cm
Screw Speed 30 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10124 / 243591

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.