Pearlitic and Martensitic. Temper carbon in necessary matrix without primary cementite or graphite. Applications include general engineering service at normal and elevated temperatures. Dimensional tolerance range for castings is stipulated. |
ASTM A220, ANSI G48.2, MIL-I-1444B, Malleable iron casting grade 90001, pearlitic, martensitic |