MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Capron® SEG6 H1 30% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Capron SEG6 H1 is a 30% glass reinforced nylon 6 injection molding compound. This material is currently under development as XA-2678. It exhibits exceptional surface aesthetics at the slower fill speeds associated with the gas assist injection molding process. It's also suitable for conventional injection molding applications in which an aesthetic surface is difficult to attain. It maintains excellent strength, stiffness, high temperature performance and dimensional stability with a high resistance to creep under load. Other attributes are: inherent chemical resistance, particularly to greases, oils and hydrocarbons; and wide processing window.

Capron SEG6 H1 is generally recommended for applications such as metal replacements, particularly thinwall parts requiring high flow.

Data provided by Allied Signal.

Processing: Max. water content 0.12%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level.

Melt Temperature: 270-295 degC (518-563 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) This product can be processed over a wide range of mold temperatures; however, for applications where aesthetics critical, a mold surface temperature of 80-95 degC (176-203 degF) is required. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Back pressure can be utilized to provide uniform melt consistency and reduce trapped air and gas. A maximum of 3.5 bar (50 psi) is recommended to minimize glass fiber breakage. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing. Surface appearance is directly affected by injection rate.

Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/ccISO data
Water Absorption 1.1 %24 hrs; ISO data
Moisture Absorption at Equilibrium 1.9 %50% RH; 23°C; ISO data
Water Absorption at Saturation 6.7 %in water; 23°C; ISO data
Linear Mold Shrinkage 0.0030 cm/cmASTM Data MD
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 160 MPaSame value from ASTM and ISO tests; 5 mm/min.
Elongation at Break 4.5 %ISO, 5 mm/min
 4.5 %ASTM, 5 mm/min
Flexural Yield Strength 245 MPaASTM Data
Flexural Modulus 8.30 GPaASTM Data
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °CASTM and ISO test
Deflection Temperature at 0.46 MPa (66 psi) 194 °CASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 214 °CASTM Data
 
Processing PropertiesOriginal ValueComments
Drying Temperature 85.0 °CSee Materials Notes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® 8202C HS PA6 (Conditioned)
BASF Ultramid® 8234G HS 44% Glass Filled PA6 (Conditioned)
Overview of materials for Nylon 6, 30% Glass Fiber Filled
BASF Ultramid® 8234G HS 44% Glass Filled PA6 (Dry)
BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Dry)

PALD65 / 23959

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.