MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Oceanchem Group Potassium Bromate (KBrO3)
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Molecular Formula: KBrO3

Cas No.: 7758-1-2

Use: This product is a strong ixidant, mainly used as chemical agent, printing and dyeing auxiliary, quality-improving reagent for wheat granules in food additive and improving reagent for tinned fish and meat.

Properties: This product is white crystal or powder. It is free of smell and tastes salty and slightly bitter. It absorbs water easily and agg lomerates in the air, but does not deliquify. It dissolves easily in water but slightly in alcohol. Its water solution is neutral.

Information Provided by Oceanchem Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.26 g/cc
Molecular Weight 167 g/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point 370 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.10 %Food Grade
 
Component Elements PropertiesOriginal ValueComments
Arsenic, As <= 0.00030 %Food Grade
Iron, Fe <= 0.00050 %Analytically pure
 <= 0.0010 %Chemically pure
Sodium, Na <= 0.020 %Analytically pure
 <= 0.050 %Chemically pure
 
Descriptive Properties
CAS Number7758-1-2
Chloride and Chlorate (%)<0.03Analytically pure; as Cl
 <0.1Chemically pure; as Cl
Content (%)>99.5Chemically pure; with KBrO3
 >99.8Analytically pure; with KBrO3
 99-101.00Food grade; with KBrO3
Content of Br (%)<0.005Analytically pure
 <0.04Chemically pure
 PassedFood grade
Degree of ClearancePassedAnalytically pure
 PassedChemically pure
Heavy Metal (%)<0.0005Analytically pure; as Pb
 <0.001Chemically pure; as Pb
Molecular FormulaKBrO3
Water-insoluble (%)<0.002Analytically pure
 <0.01Chemically pure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

POCEAN11 / 104215

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.