Availability: North America Forms: Pellets Filler/Reinforcement: Glass Fiber Reinforcement, 14% Filler by Weight Additive: Heat Stabilizer and Lubricant Features: Lubricated and Heat Stabilized Appearance: Black TPCI# 9321101 Information provided by TP Composites, Inc. |