MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SACO AEI THERMODAN® CP 0110-110 BK Lead-free Thermoplastic CPE compound
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: THERMODAN® CP 0110-110 BK is a black, UV resistant, lead-free, RoHS compliant, thermoplastic CPE compound. It is designed for use in a wide variety of jacketing applications including wire and cable and tube bundles. This compound has superior fire performance including slow flame propagation and self-extinguishing characteristics. THERMODAN® CP 0110-110 BK should be extruded with a screw configuration designed to optimize process conditions and throughput. This extrusion compound meets or exceeds several industry jacketing specifications including UL 1277 tray cable.

Information provided by SACO AEI Polymers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.41 g/ccASTM D792
Melt Flow 8.4 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
Deformation 8.0 %
@Load 0.200 kg,
Temperature 121 °C
UL 1277
Storage Temperature 4.44 - 26.7 °F
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 97
@Time 1.00 sec
ASTM D2240
Hardness, Shore D 51
@Time 10.0 sec
ASTM D2240
Tensile Strength at Break 2391 psiASTM D638
 1890 psi
@Treatment Temp. 100 °C,
Time 346000 sec
IRM 902 Oil; ASTM D638
 2080 psi
@Treatment Temp. 75.0 °C,
Time 5.18e+6 sec
After 60 days, IRM 902 Oil; ASTM D638
 2390 psi
@Treatment Temp. 121 °C,
Time 605000 sec
after thermal ageing; ASTM D638
Elongation at Break 363 %ASTM D638
 261 %
@Treatment Temp. 100 °C,
Time 346000 sec
IRM 902 Oil; ASTM D638
 287 %
@Treatment Temp. 75.0 °C,
Time 5.18e+6 sec
After 60 days, IRM 902 Oil; ASTM D638
 410 %
@Treatment Temp. 121 °C,
Time 605000 sec
after thermal ageing; ASTM D638
Flexural Modulus 19900 psi1% secant; ASTM D790
Tear Strength 342 pliASTM D470
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -23.0 °CASTM D746
Oxygen Index 34 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Zone 1 300 - 320 °F
Zone 2 320 - 345 °F
Zone 3 345 - 365 °F
Zone 4 345 - 365 °F
Die Temperature 370 - 390 °F
Melt Temperature 360 - 380 °F
Head Temperature 345 - 365 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSACO076 / 265506

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.