MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC VALOX™ FR V4860HR PBT (Americas)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: VALOX V4860HR is a 30% glass filled, impact modified, hydrolytically stable flame retardant Polybutylene Terephthalate (PBT) injection moldable grade. It has excellent chemical resistance and a UL94V0@0.80 flame rating. This is a good candidate for a variety of applications needing a sustainable FR PBT/PET solution.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.64 g/ccASTM D792
Density 1.64 g/ccISO 1183
Water Absorption 0.19 %23°C/sat; ISO 62
Moisture Absorption 0.0600 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0018 - 0.0021 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0075 - 0.0094 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 12 g/10 min
@Load 5.00 kg,
Temperature 250 °C
cm³/10 min; ISO 1133
 17.8 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 110 MPa5 mm/min; ISO 527
 114 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 111 MPa5 mm/min; ISO 527
 116 MPa5 mm/min; ASTM D638
Elongation at Break 2.1 %5 mm/min; ISO 527
 2.3 %5 mm/min; ASTM D638
Elongation at Yield 2.1 %5 mm/min; ISO 527
 2.2 %5 mm/min; ASTM D638
Tensile Modulus 9440 MPa1mm/min; ISO 527
 9750 MPa5 mm/min; ASTM D638
Flexural Strength 2.00 MPabrk, 1.3 mm/min, 50 mm span; ASTM D790
 182 MPa2 mm/min; break; ISO 178
Flexural Yield Strength 174 MPa1.3 mm/min, 50 mm span; ASTM D790
 183 MPa2 mm/min; ISO 178
Flexural Modulus 6740 MPa1.3 mm/min, 50 mm span; ASTM D790
 7870 MPa2 mm/min; ISO 178
Flexural Strain at Break 2.9 %2 mm/min; ISO 178
Izod Impact, Notched 90.0 J/mASTM D256
 74.0 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 10.0 kJ/m²80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 10.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 13.0 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 22.8 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
 23.5 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E831
CTE, linear, Transverse to Flow 114 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E831
 119 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Hot Ball Pressure Test 75.0 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 221 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 188 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 197 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 205 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 175 °CRate B/120; ISO 306
 176 °CRate B/50; ASTM D1525
 176 °CRate B/50; ISO 306
Flammability, UL94 V-0
@Thickness 0.800 mm
UL 94 by SABIC-IP
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 240 - 260 °CInjection Molding
Zone 1 220 - 240 °C
Zone 2 230 - 250 °C
Zone 3 240 - 260 °C
Melt Temperature 230 - 260 °C
Mold Temperature 60.0 - 120 °C
Drying Temperature 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 12.0 hourCumulative; Injection Molding
Moisture Content 0.020 %
Back Pressure 0.300 - 0.700 MPa
Shot Size 30 - 70 %
Vent Depth 0.00250 - 0.00380 cm
Screw Speed 20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10353 / 243820

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.