MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Epoxy Technology EPO-TEK® 302 Fast Setting, Optical Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Product Description: EPO-TEK® 302 is a two component, fast-gelling, room temperature curing epoxy, designed for electronic, optical, medical, and general applications.

Advantages & Application Notes:

  • Due to its versatility, it may be used to adhere, seal, pot or encapsulate.
  • Allows for % transmission in VIS and NIR range. It can be used as an adhesive in the optical pathway of light.
  • Convenient and easy to use 1:1 mix ratio allows for hand, meter mix, or specialty packaging.
  • Suggested applications:
  • Field Assembly: mix and cure in the field. Fast gelling and curing in 2-3 hours is accomplished.
  • Electronics: rapid prototyping of parts with fast curing epoxy – no need for oven cycle times.
  • Optics: active alignment of optics such as lenses, prisms, diodes, filters, etc. to opto-circuit.
  • Fiber Optics: “field curing” or field assembly of connectors and couplers; also suggested for fiber optic splicing.
  • Medical: adhesion to most metals, plastics, ceramics, and glasses found in tubing, substrates or housing.
  • General: arts and crafts repair, restoration, and hobbyists.

    Information Provided by Epoxy Technology

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Specific Gravity 0.900 g/ccPart B
     1.20 g/ccPart A
    Viscosity 5000 - 10000 cP
    @Temperature 23.0 °C
    20 rpm
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Shore D 73
    Tensile Modulus 154000 psiStorage
    Shear Strength >= 1700 psiDie
     1756 psiLap
     
    Electrical PropertiesOriginal ValueComments
    Volume Resistivity >= 2.00e+13 ohm-cm
    Dielectric Constant 2.95
    @Frequency 1000 Hz
    Dissipation Factor 0.010
    @Frequency 1000 Hz
     
    Thermal PropertiesOriginal ValueComments
    CTE, linear 52.0 µm/m-°CBelow Tg
     191 µm/m-°CAbove Tg
    Maximum Service Temperature, Air 100 °CContinuous
     200 °CIntermittent
    Minimum Service Temperature, Air -55.0 °CContinuous
     -55.0 °CIntermittent
    Glass Transition Temp, Tg >= 40.0 °CDynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
    Decomposition Temperature 261 °CDegradation Temperature
     
    Optical PropertiesOriginal ValueComments
    Refractive Index 1.5442
    @Wavelength 589 nm
    uncured
    Transmission, Visible >= 75 %
    @Wavelength 340 - 420 nm
    Spectral
     >= 85 %
    @Wavelength 440 - 900 nm
    Spectral
     >= 88 %
    @Wavelength 900 - 1600 nm
    Spectral
     
    Processing PropertiesOriginal ValueComments
    Cure Time 2.00 hour
    @Temperature 23.0 °C
    Pot Life 10 min
    Shelf Life 12.0 Month
    @Temperature 25.0 °C
     
    Descriptive Properties
    ColorClear/ColorlessPart A
     Clear/ColorlessPart B
    ConsistencyPourable liquid
    Mix Ratio by Weight1:1
    Number of ComponentsTwo
    Weight Loss2.68%200°C
     8.39%250°C

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3
    BCC Products BC 8782 Urethane Casting
    Silicon, Si
    Master Bond EP21TDC-4 Two Component, Highly Flexible Epoxy System
    Epoxy Technology EPO-TEK® OG603 UV Cure Optical Epoxy

    PPOXYT109 / 141148

    Ensinger PEI

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.