MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRICOMP™ Compound EFL36 Polyetherimide (PEI) (Europe)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: LNP LUBRICOMP EFL36 compound is based on Polyetherimide (PEI) resin containing 30% glass fiber, 15% PTFE. Added features of this grade include: Wear Resistant.

Features: Wear resistant,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.62 g/ccISO 1183
Water Absorption 0.32 %
@Time 86400 sec
ISO 62-1
Moisture Absorption 0.0200 %Injection Molding
 0.180 %23°C / 50% RH; ISO 62
Viscosity 3.0 - 5.0 cP
@Load 5.00 kg,
Temperature 345 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.00060 cm/cm24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0026 cm/cm24hrs; ISO 294
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 168 MPaISO 527
Elongation at Break 2.0 %ISO 527
Flexural Strength 216 MPayield, 2 mm/min; ISO 178
 85.0 MPa
@Temperature 200 °C
yield, 2 mm/min; ISO 178
 141 MPa
@Temperature 150 °C
yield, 2 mm/min; ISO 178
 167 MPa
@Temperature 120 °C
yield, 2 mm/min; ISO 178
 182 MPa
@Temperature 80.0 °C
yield, 2 mm/min; ISO 178
Flexural Modulus 9000 MPa2 mm/min; ISO 178
 7300 MPa
@Temperature 200 °C
2 mm/min; ISO 178
 8100 MPa
@Temperature 150 °C
2 mm/min; ISO 178
 8200 MPa
@Temperature 120 °C
2 mm/min; ISO 178
 8500 MPa
@Temperature 80.0 °C
2 mm/min; ISO 178
Flexural Strain at Break 2.7 %2 mm/min; ISO 178
 2.0 %
@Temperature 200 °C
2 mm/min; ISO 178
 2.5 %
@Temperature 150 °C
2 mm/min; ISO 178
 2.5 %
@Temperature 80.0 °C
2 mm/min; ISO 178
 2.6 %
@Temperature 120 °C
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²80*10*4; ISO 180/1A
 10.0 kJ/m²
@Temperature -40.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) 35.0 kJ/m²80*10*4; ISO 180/1U
 35.0 kJ/m²
@Temperature -40.0 °C
80*10*4; ISO 180/1U
Impact Test 3.00 JMultiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.45ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.43ASTM D3702 Modified: Manual
K (wear) Factor 35.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 175 - 250 VUL 746A
Hot Wire Ignition, HWI >= 120 sec
@Thickness >=0.750 mm
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
@Thickness >=0.750 mm
UL 746A
 15 - 30 arcs
@Thickness >=3.00 mm
UL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 28.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 40.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Specific Heat Capacity 1.307 J/g-°CASTM E1269
Thermal Conductivity 0.230 W/m-KASTM D5930
Deflection Temperature at 1.8 MPa (264 psi) 204 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
UL RTI, Electrical 180 °CUL 746B
UL RTI, Mechanical with Impact 170 °CUL 746B
UL RTI, Mechanical without Impact 180 °CUL 746B
Flammability, UL94 V-0
@Thickness >=0.750 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 365 - 375 °C
Zone 2 360 - 370 °C
Zone 3 365 - 375 °C
Melt Temperature 360 - 375 °CInjection Molding
Mold Temperature 140 - 180 °C
Drying Temperature 150 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa
Vent Depth 0.00250 - 0.00760 cm
 
Descriptive Properties
Screw speed (Circumferential speed)0.2-0.3 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80774 / 288721

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.