Turco 6783-10 is an aqueous compressor cleaner which effectively removes oil, salt and solid deposits from compressor blades, guide vanes and rotors of in-service turbine engines. Periodic cleaning of these components is necessary to avoid power loss, abnormal temperature increases, increased fuel consumption and excessive NOx emissions. Supplied in a Ready-to-Use liquid form. Meets MIL-C-85704B Type II and III. |
Aerospace Surface Treatment |